What is the raw material
Super Raw Material | |||
HRC 45 | HRC 55 | HRC 60 | HRC 65 |
YG10X | YL10.2&WF25 | Germany K44&K40 | Sandvik H10F |
Grain size 0.7 μm,Co10%,Flexural strength 3320N/mm² | Grain size 0.6 μm,Co10%,Flexural strength 4000N/mm² | Grain size 0.5 μm,Co12%,Flexural strength 4300N/mm² | Grain size 0.5 μm,Co10%,Flexural strength 3320N/mm² |
Super Coating | |||||
Coating | Hardness HV | Thickness μm | Friction Coefficient | Oxidation Temp | Color |
AlTiN | 3500 | 2.5-3 | 0.3 | 900 | Black |
TiAlN | 2800 | 2.5-3 | 0.3 | 900 | Violet |
TiSiN | 3600 | 3 | 0.45 | 1000 | Bronze |
AlTiSiN | 4000 | 3 | 0.4 | 1200 | Blue |
TiN | 2500 | 2-3 | 0.5 | 600 | Gold |